PRODUCTION
Changzhou Strengh Power Technology Co.Ltd
CR2032-5B
The company mainly produces over 50 varieties of alkaline batteries, carbon batteries, button type lithium manganese batteries, and other products, which are widely used in electronic appliances such as automobiles, computer motherboards, remote controls, and so on
Keywords: alkaline battery | button type lithium manganese battery | carbon battery
Category:
Model:
CR2032
Standard:
3V
Product Size:
20(D)*3.2(H)
mm
Weight:
3g
Package:
Shrink/hang card
Certification:
CE,ROHS,SGS,REACH,UL,KC,UN38.3,MSDS
E-mail:zoey@anyida-power.com
Tel:0519 -83270441
Detailed description
Daily-max: |
CR2032 |
IEC: |
CR2032 |
Maxell: |
CR2032 |
SONY: |
CR2032 |
DURACELL: |
DL2032 |
2. Battery type and ratings
Electrochemical System |
Lithium manganese dioxide/organic electrolytes |
||
Nominal Voltage |
3V |
||
Nominal Capacity (Continuous Discharging Under 15kΩ load to 2.0V End-Voltage at 20℃) |
210mAh |
||
Operating temperature range |
-20℃~70℃ |
||
|
diameter(A) |
20.0(-0.3)mm |
|
|
height(B) |
3.2(-0.3)mm |
|
Mass |
Approx2.8g |
||
Appearance and poles |
Appearance should be smooth, clear mark, no deformation, rust, and leakage |
||
minimum average duration (Load 15kΩ) |
Initial test (New battery in 60 days) |
1000h |
|
|
After 12 months |
950h |
|
Open Voltage |
Initial test (New battery in 60 days) |
3.10V-3.45V |
|
|
After 12 months |
3.10V-3.45V |
|
Closed Circuit Voltage(15kΩ) |
Initial test (New battery in 60 days) |
3.10V-3.45V |
|
|
After 12 months |
3.00V-3.45V |
|
Leakage Characteristics (Over discharge) |
No Leakage |
3.Test Method
|
Item |
Condition |
1 |
Dimensions |
When measure with vernier calipers which precision is up 0.02mm. to avoid short circuit, should paste on one insulation material on one end of the vernier calipers. |
2 |
Open voltage |
the precision of multimeter is not lower than 0.25%, intel resistance is bigger than 1MΩ |
3 |
Instant short-circuit current |
When test with multimeters, not surpass 0.5 second each time, avoid duplicating tests, if need once more, the time-gap should above half hour |
4 |
Appearance |
Appearance of batteries shall be inspected by visual means. |
5 |
Min time of discharge |
Lay aside above 8 hours in the temperature of 20±2℃ and under the humidity of 60±15% conditions, with the condition that Resistance is 15kΩ, end-point voltage is 2.0V. The new battery (Initial stage) should be tested in 60 days after produce. The old battery (Delayed for 12 months) should be tested in 14 days after the storage period. |
6 |
Over-discharge Characteristics |
Take nine battery in the temperature of 20±2℃ and under the humidity of 60±15% conditions, with the condition that Resistance is 15kΩ, end-point voltage is 1.2V. visual test. |
|
Check item |
IL |
AQL |
1 |
Dimensions |
I |
0.25 |
2 |
Open voltage |
|
0.25 |
3 |
Appearance |
Ⅱ |
0.25 |